Product Description: Exact 9371 plastomer is an ethylene butene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties. Key Features: - PP/TPO modification.
- EVA modification.
- Designed as a low density and high molecular weight polymer modifier to impart impact strength and toughness.
- Available as free flowing pellets.
Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaAll physical properties were measured from specimens cut from compression molded plaques per ASTM D 4703, Procedure A, Type I and conditioned at 23°C for a minimum of 40 hours per ASTM D 618 prior to testing.
All stress/strain tests used specimens cut with a Type IV (Die C) die and tested with a grip separation of 25 mm (1") and a crosshead speed of 20 in./min. Information provided by ExxonMobil Chemical. |