MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Kraton® D1119 P (SIS) Linear Block Copolymer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Description: Kraton D1119 P is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 22%. It is supplied from North America in the physical form identified:
Kraton D1119 PT - supplied as a dusted dense pellet
Kraton D1119 PSM - supplied as a powder dusted with silica

Region: Asia Pacific, Europe, Japan, North America, and South America

Uses: Kraton D1119 P is used as an ingredient in formulating adhesives, sealants and coatings. It may also find use as a modifier of bitumen or thermoplastics and in compound formulations.

Applications: Adhesives, Sealant and Coatings; Compounding and Personal Hygiene; Impact Modification; Footwear; and Bitumen Modification

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.930 g/cc0.930 g/ccASTM 4025
Volatiles <= 0.50 %<= 0.50 %KM 04
Melt Flow 25 g/10 min
@Load 5.00 kg,
Temperature 200 °C
25 g/10 min
@Load 11.0 lb,
Temperature 392 °F
Ash 0.30 - 0.40 %0.30 - 0.40 %Talc; BAM 908
 2.5 - 5.0 %2.5 - 5.0 %The final dusting level is a combination of the talc from the original D1119 PT and silica added during the milling process; ISO 247
 
Chemical PropertiesMetricEnglishComments
Diblock Content 66 %66 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 303010 seconds. Typical values on polymer compression molded at 150°C (300°F).; ASTM 2240
Tensile Strength, Ultimate 2.41 MPa350 psiTypical properties based on film cast from toluene solution.; ASTM D412
Elongation at Break 1000 %1000 %Typical properties based on film cast from toluene solution.; ASTM D412
300% Modulus 1.00 MPa
@Strain 300 %
145 psi
@Strain 300 %
film cast from toluene solution.; ASTM D412
 
Descriptive Properties
ContentAntioxidant0.08-0.3%, KM 08
 Polystyrene20.5-23.5%, KM 03
 Total Extractables<1.0%, KM 05
Styrene/Rubber ratio22/78

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kraton® G1650 E (SEBS) Linear Block Copolymer
Kraton® D4141 (SBS) Linear Block Copolymer
Kraton® D1101 (SBS) Linear Block Copolymer
Kraton® D1107P (SIS) Linear Block Copolymer
Kraton® D1112P (SIS) Linear Block Copolymer

PKRA0100 / 49070

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.