MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP 6002-45A Specialty Thermoplastic Elastomer, Bondable to PC/ABS, PC, ABS  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes:


Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.980 g/ccASTM D792
Linear Mold Shrinkage 0.030 cm/cm
@Thickness 3.17 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 4510 sec; ASTM D2240
Tensile Strength at Break 1200 psiASTM D412
Tensile Strength, Yield 150 psi50%; ASTM D412
 200 psi100%; ASTM D412
 420 psi300%; ASTM D412
Elongation at Break 1100 %ASTM D412
Tear Strength 150 pliDie C; ASTM D624
Peel Strength 20.0 pliABS; Failure Type D; 90 degrees, 20 in/min (500 mm/min); ISO 813
 24.0 pliPC; Failure Type D; 90 degrees, 20 in/min (500 mm/min); ISO 813
 27.0 pliPC/ABS; Failure Type D; 90 degrees, 20 in/min (500 mm/min); ISO 813
Compression Set 27 %22 h 23 °C (73 °F); Method B Type 2; ASTM D395
 71 %22 h 70 °C (158 °F); Method B Type 2; ASTM D395
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 HB
@Thickness 1.59 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 380 - 460 °F
Mold Temperature 70.0 - 120 °F
Drying Temperature 170 °F2 - 4 hrs
Moisture Content 0.040 %
Injection Pressure 5000 - 15000 psi

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teknor Apex Monprene® MP-2207B Thermoplastic Elastomer
Polymax® Maxelast® A9945T TPE, ABS/PC Overmold
Polymax® Maxelast® A9845 TPE, ABS/PC Overmold

PQZXA1000 / 58456

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.