Product Description: Riteflex 855 is polyester thermoplastic elastomer with high melt strength and nominal Shore D hardness of 55D. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Material Status: Experimental Information provided by Celanese |