MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger Tecapeek® CLASSIX XRO Polyetheretherketone (PEEK)
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: TECAPEEK™ high performance polymer, made from Victrex PEEK polymer, has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's exceptional combination of properties allow engineers and designers the ability to create cost-effective, innovative parts that exhibit outstanding wear, heat, electrical and chemical resistance. The TECAPEEK™ family is made up of materials for medical applications.

  • TECAPEEK™ MT, unfilled pigmented medical grade PEEK
  • TECAPEEK™ XP98, compression molded 30% carbon fiber filled PEEK (isotropic properties)
  • TECAPEEK™ MT CF30, extruded 30% carbon fiber filled PEEK
  • TECAPEEK™ Classic™, ISO 10993 certification by resin and extrusion lot of 30 days contact
  • TECAPEEK™ Classix™ XRO-20 radio opaque grade with 20% BaSO4 added

The TECAPEEK™ family of high performance plastics are high effective in the creation and manufacture of high quality medical instruments.

Information Provided by Ensinger Industries, Inc.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

TriStar Plastics Corp. provides engineering, custom fabrication and manufacturing of high-performance plastics and self-lubricating bearing materials, such as Rulon, PEEK, Torlon, CJ Composites and Ultracomp. Capabilities include component design, material selection, prototype and production, manufacturing and surface modification. Call (800) TRI-STAR (800) 874-7827 or visit or www.TStar.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.65 g/ccASTM D792
Density 0.0596 lb/in³ASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 11600 psi
@Temperature 22.8 °C
ASTM D638
Elongation at Break 2.0 %ASTM D638
Tensile Modulus 725000 psi
@Temperature 22.8 °C
1% Secant; ASTM D638
Flexural Modulus 580000 psi
@Temperature 22.8 °C
ASTM D790
 
Thermal PropertiesOriginal ValueComments
Melting Point 644 °F
Maximum Service Temperature, Air 500 °Fcontinuous

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyetheretherketone, Unreinforced
Ensinger Tecapeek® Polyetheretherketone (PEEK)
Ensinger Tecapeek® MT Polyetheretherketone (PEEK)
Ensinger Tecapeek® GF30 Polyetheretherketone, 30% Glass Reinforced (PEEK)
Ensinger Tecapeek® MT CF 30 Polyetheretherketone (PEEK)

PENSIN026 / 92843

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.