MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BEC Materials SBS 185
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: Description: Thermoplastic elastomer SBS rubber 185 is oil-extended, radiation type, styrene-butadiene-styrene triblock copolymer. Its oil-filled rate is 31%, and styrene content is 32%. It can be injection molded directly due to its high fluidity.YH-185 and YH-815 are both radiation type oil-extended rubber. However the wear-resisting property and tensile strength of SBS polymer YH-185 have been significantly improved than YH-185.

Application: Adhesives/Shoes/Compounding

Formula: TPR Shoe (Parts by mass)
SBS(YH185): 130
Oil: 45
PS: 15
CaCO3: 75

Information provided by BEC Materials, LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 0.70 %
Melt Flow 0.10 - 2.0 g/10 min
 
Chemical PropertiesOriginal ValueComments
Styrene Content 32 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 60 - 70
Tensile Strength >= 15.0 MPa
 
Descriptive Properties
Oil Content0.31

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBECM049 / 307002

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.