MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Trivalence Technologies Polymers

Trivalence Technologies TriBLEND 22G10 (U,R) Polycarbonate + PBT
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: Polycarbonate + PBT, medium flow, available with UV and/or release, 10% glass reinforced

Typical Applications: Military, lawn & garden, automotive, electronics, medical devices, housings

Information provided by Trivalence Technologies.

Vendors: Trivalence Technologies offers solution driven Custom Compounding, Distribution and Applied Sciences to the world’s plastic injection and extrusion markets. We pair our leading-edge resins and blends with personal attention to each customer’s needs. We work with you one-on-one at every stage and at every level to make sure you have an exceptional experience every time. Click to view more about the services we offer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³ASTM D792
Linear Mold Shrinkage, Flow 0.0050 - 0.0080 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0080 in/in
@Thickness 0.126 in
TVT Internal Test
Melt Flow 28 g/10 min
@Load 5.00 kg,
Temperature 260 °C
28 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 109109ASTM D785
Tensile Strength, Yield 75.8 MPa11000 psiASTM D638
Flexural Modulus 3.79 GPa550 ksiASTM D790
Izod Impact, Notched 0.961 J/cm1.80 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 193 °C380 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 157 °C315 °FASTM D648
Vicat Softening Point 152 °C305 °FASTM D785
Flammability, UL94 HB
@Thickness 1.52 mm
HB
@Thickness 0.0600 in
TVT Internal Test
 
Processing PropertiesMetricEnglishComments
Melt Temperature 254 - 277 °C490 - 530 °F
Mold Temperature 65.6 - 87.8 °C150 - 190 °F
Drying Temperature 93.3 - 116 °C
@Time 7200 - 14400 sec
200 - 240 °F
@Time 2.00 - 4.00 hour
Moisture Content 0.020 %0.020 %
 
Descriptive Properties
AvailabilityAsia
 Europe
 Latin America
 North America
CharacteristicInjection/Extrusion
ColorAll, Opaque/Translucent
FillerGlass Fiber
FormPellets
Outdoor Suitability (QUV)PassTVT Internal Test, "U" Grade

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTRIV9510 / 313865

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.