MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Navy "M" Bronze, UNS C92200, Copper Casting Alloy, M02 Temper, As Centrifugal Cast
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Temper: As Centrifugal Cast

Casting Characteristics: High – Effect of Section Size; Medium – Fluidity, Casting Yield, Gassing; Low - Drossing, Shrinkage in Solidification

Fabrication Properties: Excellent Suitability – Soldering, Brazing

Typical uses: Ornamental Castings; Cooling Equipment; Heating Equipment; Nuts; Bearings; Bushings; Cryogenic Valves; Fittings Used to 550 F; Gears; Medium Pressure Hydraulic Equipment; Piston Rings; Pump Impellers; Pumps Used to 550 F; Valve Components; Valves for Water Meters; Marine Castings; Medium Pressure Steam Equipment to 550 F

Applicable Specifications: As Centrifugal Cast – Castings ASTM B271/B271M, Castings SAE J461, Castings SAE J462; As Continuous Cast – Castings SAE J462, Castings SAE J461, Castings ASTM B505/B505M; As Sand Cast – Castings SAE J462, Castings SAE J461, Castings ASTM B584, Castings ASTM B61, Castings ASME SB584, Castings ASME SB61; Fitting – ASME SB61, ASTM B61, FEDERAL WW-P-460, ASME B16.24; Flanges ASTM B61, ASME SB61, FEDERAL WW-P-460; Ingot - ASTM B30; Valves MILITARY MIL-V-17547

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.312 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 34.0 ksifor Standard
Tensile Strength, Yield >= 16.0 ksifor Standard, 0.5% Ext
Elongation at Break >= 22 %for Standard
Tensile Modulus 14000 ksi
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000123 ohm-cm14% IACS
Magnetic Permeability 1.0
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.0 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.0900 BTU/lb-°F
Thermal Conductivity 40.2 BTU-in/hr-ft²-°F
Melting Point 600 °FIncipient
 1518 - 1810 °F
Solidus 1518 °F
Liquidus 1810 °F
Shrinkage 1.56 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.0050 %
Antimony, Sb <= 0.25 %
Copper, Cu 86 - 90 %
Iron, Fe <= 0.25 %
Lead, Pb 1.0 - 2.0 %
Nickel, Ni <= 1.0 %
Phosphorus, P <= 0.050 %
Silicon, Si <= 0.0050 %
Sulfur, S <= 0.050 %
Tin, Sn 5.5 - 6.5 %
Zinc, Zn 3.0 - 5.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC92200x1 / 293204

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.