MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Shell Carilon® D26CX100 Polyketone, Advanced Extrusion Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polyketone

Material Notes: Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer D26CX100 is an extrusion grade with mechanical properties that classify it as an engineering thermoplastic. This grade combines high melt strength and viscosity with high chemical resistance and barrier performance. Moreover, this material exhibits a high impact resistance, both at room temperature and at lower temperatures, and good creep performance. CARILON Polymer D26CX100 can also withstand short-term exposure to elevated temperatures. CARILON Polymer D26CX100 has been designed for demanding extrusion processes. This grade should be considered for liners, pipes and large blow moldings.

Data provided by Shell Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.24 g/ccASTM D792
Water Absorption 0.45 %24 hour immersion; ASTM D570
Moisture Absorption at Equilibrium 0.53 %at 50% RH; ASTM D570
Water Absorption at Saturation 2.1 %ASTM D570
Melt Flow 2.7 g/10 min
@Load 2.16 kg,
Temperature 240 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 63.0 MPaASTM D638
Tensile Strength, Yield 59.0 MPaASTM D638
Elongation at Break 230 %ASTM D638
Elongation at Yield 25 %ASTM D638
Tensile Modulus 1.60 GPaASTM D638
Flexural Modulus 1.60 GPaASTM D790
Izod Impact, Notched 2.70 J/cm
Izod Impact, Unnotched NBASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 °C
Deflection Temperature at 0.46 MPa (66 psi) 210 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 105 °CASTM D648
Vicat Softening Point 210 °CASTM D1525
 
Processing PropertiesOriginal ValueComments
Processing Temperature 240 °CAt Die

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Ketron® LSG PEEK, Extruded Unfilled Polyetherether Ketone (ASTM Product Datasheet)
Shell Carilon® DP R1000 Polyketone
Shell Carilon® DP P1000 Polyketone
Shell Carilon® D26HM100 Polyketone, General-Purpose Injection Molding Grade
Shell Carilon® D26FX100 Polyketone, General-Purpose Extrusion Grade

PCAR03 / 27912

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.