MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Chromium-Copper, UNS C17600, TB00 Temper rod, bar, wire, tubing, plate, forged products
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Applications: resistance welding electrodes for spot, seam, flash, and projection welding methods; electrical connectors, clips

TB00 temper rod, bar, wire, plate, tubing, and forged products.

Inactive per the Copper Development Association.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.75 g/cc0.316 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 25 - 4525 - 45Forged products
 20 - 5020 - 50Rod, bar, wire, tubing, plate
Tensile Strength, Ultimate 240 - 380 MPa34800 - 55100 psi
Tensile Strength, Yield 140 - 205 MPa
@Strain 0.2 %
20300 - 29700 psi
@Strain 0.2 %
Elongation at Break 20 - 35 %20 - 35 %
Modulus of Elasticity 125 - 130 GPa18100 - 18900 ksi
Shear Modulus 44.0 GPa6380 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000287 - 0.00000862 ohm-cm0.00000287 - 0.00000862 ohm-cm
 0.0000057 - 0.0000086 ohm-cm
@Temperature 20.0 °C
0.0000057 - 0.0000086 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.7 µm/m-°C
@Temperature 20.0 - 200 °C
9.28 µin/in-°F
@Temperature 68.0 - 392 °F
Specific Heat Capacity 0.420 J/g-°C0.100 BTU/lb-°F
Thermal Conductivity 215 - 245 W/m-K1490 - 1700 BTU-in/hr-ft²-°F
Melting Point 1031 - 1068 °C1888 - 1954 °F
Solidus 1031 °C1888 °F
Liquidus 1068 °C1954 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 975 °C1790 °FHot-Shortness Temperature
Annealing Temperature 900 - 950 °C1650 - 1740 °F10 minutes/water quench
Aging Temperature 425 °C797 °F3-6 hours, for maximum strength
 480 °C896 °FCommercial practice, 2-3 hours
Hot-Working Temperature 750 - 925 °C1380 - 1700 °F
 
Component Elements PropertiesMetricEnglishComments
Beryllium, Be 0.25 - 0.50 %0.25 - 0.50 %
Co + Ni >= 1.4 %>= 1.4 %
Co + Ni + Fe <= 1.9 %<= 1.9 %
Cobalt, Co 1.4 - 1.7 %1.4 - 1.7 %
Copper, Cu 97 %97 %
Silver, Ag 0.90 - 1.1 %0.90 - 1.1 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Copper-Cobalt-Beryllium alloy, UNS C17500, TB00 Temper strip, rod, bar, plate, tubing, forged products
Ampco Metal AMPCOLOY® 89 Beryllium Copper, Extrusion
Beryllium Copper, UNS C17300, TB00 Temper Strip
Beryllium Copper, UNS C17200, TB00 Temper Strip
Beryllium Copper, UNS C17000

MC17600b1 / 10902

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.