Nitrile Butadiene/PVC Rubber, 65-75 °IRHD. Copolymer of acrylonitrile and butadiene blended with PVC. Applications: Excellent resistance in sealing applications against petroleum and mineral based fuels and oils. Compounded with PVC to provide improved resistance to ozone and weathering. |