MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CHT Group Magnifoam™ MFSILTEC™ Roll Stock MTI Silicones Silicone Foam
Categories: Polymer; Thermoset; Silicone; Silicone Foam

Material Notes: Part of the Amber Chemical Group. Data provided by manufacturer.

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 12.0 lb/ft³ASTM D1056
Water Absorption 3.0 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 30.0 psiASTM D412
Elongation at Break 100 %ASTM D412
Compressive Strength 4.00 psi25%; ASTM D3675
Compression Set <= 10 %
@Temperature 100 °C
at 50%, 22 hrs; ASTM D1056
 2.0 %
@Temperature 70.0 °C,
Time 79200 sec
at 50%; ASTM D1056
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 V-1Dependent on color and thickness
 V-0Dependent on color and thickness
Flammability Test <= 25ASTM E162/D 3675
Smoke Density 1.5 min<20; ASTM E662
 4.0 min<50; ASTM E662
 
Descriptive Properties
Thermal Resistance, ft2-h/BTU2.5ASTM C518
Toxic Gas Emission PassBombardier SMP 800C
Vertical FlammabilityPassFAR25.83(a)(1)(i) 12sec
 PassFAR25.83(a)(1)(i) 60sec

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Silicone Foam
BASF Neopolen® 1710 40 mm Expanded Polyethylene
BASF Neopolen® 1712 100 mm Expanded Polyethylene
BASF Neopolen® 1710 60 mm Expanded Polyethylene
BASF Neopolen® 1710 50 mm Expanded Polyethylene

PACC078 / 22205

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.