MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ND Industries StudGrade® 146 Permanent StudGrade HD Threadlocker
Categories: Polymer; Adhesive; Thermoset

Material Notes: General Description

High strength, high viscosity threadlockers for maximum security. Suitable for most applications where disassembly is not required.

Typical Uses

Fasteners over 1" diameter with coarse threads

Meets military spec MIL-S-46163 Type I Grade L

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 6000 - 8000 cP6000 - 8000 cP
 
Mechanical PropertiesMetricEnglishComments
Impact Test 22.6 - 33.9 J16.7 - 25.0 ft-lbPrevail
 28.2 - 39.5 J20.8 - 29.2 ft-lbBreak
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 149 °C300 °F
Minimum Service Temperature, Air -53.9 °C-65.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 10.0 min0.167 hourWith Primer (Fixture)
 60.0 min1.00 hourOn steel (fixture)
 1440 min24.0 hourOn steel (Full)
 1440 min24.0 hourWith Primer (Full)
 
Descriptive Properties
ColorRed
Gap Fill, in.0.01

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNDIND06 / 54756

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.