MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Titanium Ti-13V-2.7Al-7Sn-2Zr, ST 815°C, Aged 580°C
Categories: Metal; Nonferrous Metal; Titanium Alloy; Beta Titanium Alloy

Material Notes: ST=solution Treated

Characteristics:

  • Martensitic alloy
  • High hardenability
  • Heat treatable
  • Good fatigue properties
  • Good fracture properties
  • Suitable for hot-working and cold-forming
  • Good castability and weld repair

5 other heat treatments of this alloy are in MatWeb.

Key Words: Transage 175
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 4.70 g/cc0.170 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 1210 MPa175000 psi
Tensile Strength, Yield 1120 MPa162000 psi
Reduction of Area 10 %10 %
Modulus of Elasticity 105 GPa15200 ksiSample was ST 815ºC, Aged 540ºC
Poissons Ratio 0.330.33Typical for beta titanium alloy.
Fatigue Strength 378 MPa
@# of Cycles 1.00e+6
54800 psi
@# of Cycles 1.00e+6
unnotched
Shear Modulus 39.5 GPa5730 ksiCalculated from typical values.
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000150 ohm-cm0.000150 ohm-cmEstimated from similar high-V-stabilized beta titanium alloys.
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.50 µm/m-°C
@Temperature 20.0 - 100 °C
4.72 µin/in-°F
@Temperature 68.0 - 212 °F
Typical beta titanium alloy
Specific Heat Capacity 0.525 J/g-°C0.125 BTU/lb-°FTypical value for titanium alloys.
Thermal Conductivity 7.80 W/m-K54.1 BTU-in/hr-ft²-°FEstimated from similar high-V-stabilized beta titanium alloys.
Beta Transus 750 °C1380 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 2.7 %2.7 %
Boron, B <= 0.030 %<= 0.030 %
Carbon, C <= 0.080 %<= 0.080 %
Hydrogen, H <= 0.015 %<= 0.015 %
Iron, Fe <= 0.20 %<= 0.20 %
Nitrogen, N <= 0.050 %<= 0.050 %
Other, each <= 0.10 %<= 0.10 %
Other, total <= 0.40 %<= 0.40 %
Oxygen, O <= 0.15 %<= 0.15 %
Tin, Sn 7.0 %7.0 %
Titanium, Ti 75 %75 %
Vanadium, V 13 %13 %
Yttrium, Y <= 0.0050 %<= 0.0050 %
Zirconium, Zr 2.0 %2.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Titanium Ti-13V-11Cr-3Al (Ti-13-11-3) Aged 490°C
Titanium Ti-13V-11Cr-3Al; (Ti-13-11-3) Annealed 850°C (1560°F) + Aged 510°C 8 hr
Titanium Ti-13V-2.7Al-7Sn-2Zr, ST 815°C, Aged 510°C
Titanium Ti-13V-2.7Al-7Sn-2Zr, ST 815°C, Aged 540°C (1000°F)
Titanium Ti-13V-11Cr-3Al (Ti-13-11-3) SolnTreat; Age 450°C

MTB332 / 14189

Metalmen Sales

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.