MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CoorsTek Alumina-Zirconia Composite, AZ-25
Categories: Ceramic; Oxide; Aluminum Oxide; Zirconium Oxide

Material Notes: Information provided by CoorsTek.

Key Words: Zirconium Oxide, Aluminum Oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.82 g/ccASTM C20
Water Absorption 1.0 %ASTM C373
Particle Size 5.0 µmAverage Crystal Size - Thin Section Test
 
Mechanical PropertiesOriginal ValueComments
Knoop Microhardness 10.41000 g load
Hardness, Rockwell 45 N 75GPa
Flexural Strength 172 MPaASTM F417
Compressive Strength 2310 MPaASTM C773
Fracture Toughness 5.00 - 6.00 MPa-m½Notched Beam
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 1.00e+13 ohm-cmASTM D1829
 <= 1000 ohm-cm
@Temperature 1000 °C
ASTM D1829
 5.00e+7 ohm-cm
@Temperature 500 °C
ASTM D1829
Dielectric Constant 9.8
@Frequency 1e+6 Hz
Dielectric Loss Index 0.0010
@Frequency 1e+6 Hz
ASTM D2520
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.50 µm/m-°C
@Temperature 25.0 - 1000 °C
ASTM C372
Thermal Conductivity 13.0 W/m-KASTM C408
Maximum Service Temperature, Air 1400 °CNo Load

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CoorsTek Zirconia-Toughened Alumina, ZTA
Astro Met ZTA 96 Zirconia Toughened Alumina
Aremco AREMCOLOX™ 502-1900-ZTA Dense Zirconia-Toughened Aluminum Oxide
CeramTec 950 Zirconia Toughened Alumina (ZTA), Al2O3•ZrO2
China-Yixing Longly Refractories ZTA (20%ZrO2) Zirconia Toughened Alumina Composite Ceramic

CZ3CA / 2753

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.