MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
ASI® M 5 Cyanoacrylate Super Glue for Metal Bonding
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: Metal bonding instant adhesives used to bond metal to metal and metal to other substrates. Available in a complete range of products, the M Series has superior tensile and shear strength. With varying viscosities these methyl based cyanoacrylate adhesives, have good gap filling properties. Handling strength in most applications is in 10 seconds. M 5 is a low viscosity, wicking grade, methyl based cyanoacrylate adhesive. It is designed to bond a wide range of similar and dissimilar materials involving metal. Handling strength in most applications is in 5 to 10 seconds.

Substrates bonded include ABS, Acrylic, Aluminum, Bakelite, Brass, Chloroprene, Chrome, Cooper, EPDM, Fiberglass, Latex, Leather, Natural Rubber, NBR, Neoprene, Nitrile, Nylon, Phenolic, Polycarbonate, Polyester, Polystyrene, Porcelain, PVC, SBR, Steel, Valox, and Wood.

Information provided by Adhesive Systems, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.07 g/cc
Viscosity 5.0 cP
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 1800 psivs. Steel; ISO 6922
Adhesive Bond Strength >= 750 psiNeoprene substrate. Fixture time < 5 sec; ISO 4587
 >= 850 psiPhenolic substrate. Fixture time < 15 sec; ISO 4587
 >= 900 psiABS substrate. Fixture time < 15 sec; ISO 4587
 >= 900 psiPVC substrate. Fixture time < 10 sec; ISO 4587
 >= 900 psiPolycarbonate substrate. Fixture time < 20 sec; ISO 4587
 >= 1750 psiAluminum substrate. Fixture time < 15 sec; ISO 4587
 >= 2100 psiSteel substrate. Fixture time < 20 sec; ISO 4587
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.00e+15 - 1.00e+16 ohm-cmASTM D257
Dielectric Constant 2.0 - 3.5
@Frequency 1000 Hz
ASTM D150
Dissipation Factor <= 0.020
@Frequency 1000 Hz
ASTM D 150
 
Descriptive Properties
BaseMethyl
Color / appearanceOpaque / slight amber
Strength Retained100%. Aged 500 hrs, Ethanol @ 22°C.
 100%. Aged 500 hrs, Freon TA @ 22°C.
 100%. Aged 500 hrs, gasoline @ 22°C.
 100%. Aged 500 hrs, isopropanol @ 22°C.
 100%. Aged 500 hrs, Motor oil @ 40°C.
 100%. Aged 500 hrs, Polycarbonate @ 40°C & 95% RH.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASINC9026 / 233393

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.