MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik Protectosil® 300S Surface Treatment
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: Product Description: A clear, penetrating, breathable VOC-compliant surface treatment for use on concrete. The Isobutylakoxy functional silane allows for faster dry times and superior performance on high quality mix designs typical of new bridge decks. Creates a deep hydrophobic layer that prevents water and waterborne contaminants from entering the substrate and causing premature deterioration. By combining ultra-low surface tension with a tailored rate of reaction, Protectosil 300S is able to move through the moisture boundary layer that lines the pore structure of the substrate. This permits the development of uniform gradient permeation—a consistent level of protection throughout the entire depth of penetration—allowing for longer treatment life, especially on wearing surfaces.

Applications: For use on cast-in-place, precast, GFRC and high-strength concrete, to protect the reinforcing steel from corrosion due to the effects of water, deicing salts another waterborne contaminates. Alleviates deterioration of concrete due to alkali-silica reactivity. For use on bridge decks where fast drying is needed to minimize lane closures. For treating heavy-traffic wearing surfaces or areas that receive high salt concentrations (piers, coastal buildings), to provide a high-performance, long-lasting chloride screen.

Advantages: PROTECTOSIL 300s IS SOLVENT-FREE, Isobutylalkoxysilane. Protectosil 300S penetrates deeper than traditional silane and siloxane solvent-or water-carried systems. This deeper penetration gives a long-lasting, resistance against water and chloride intrusion. Protectosil 300S’s breathable system greatly reduces the amount of water that enters a substrate, thus promoting a “drying out” of the substrate. Reduces the deteriorating effects of water, such as alkali silica reactivity. By incorporating Protectosil 300S into your integrated design, you can earn vital Leadership in Energy & Environmental Design (LEDD) credits for both new and existing construction projects. The main benefits of the product are:

  • Excellent resistance to chloride ion ingress
  • 100% Moisture vapor transmission
  • Mitigation of AAR&ASR deterioration
  • Deep penetration into substrate
  • No change in surface appearance
  • No change in surface friction after application
  • High resistance to alkali attack
  • Long service life
  • Excellent performance on wearing surfaces
  • Quick Dry time after application(1 Hour)
  • Will not inhibit adhesion of paints and line striping

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.875 g/cc0.0316 lb/in³
Volatile Organic Compounds (VOC) Content 390 g/l390 g/l
 
Thermal PropertiesMetricEnglishComments
Flash Point 63.0 °C145 °F
 
Descriptive Properties
Colorwater white
Content>98%active

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Cos46 Cork/Synthetic Rubber Sheet
Aremco Quartz-Coat™ 845-D / 845-S High Temperature Specialty Coatings Inorganic, Silicon Filled
Evonik Protectosil® AQUA-TRETE® BHN Surface Treatment
Hippe SI GC 201 Woven Glass Cloth Reinforced Silicone Resin - Sheet
Titanium Aluminum Nitride (TiAlN) PVD Coating

PEVONIM118 / 197322

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.