MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Makrolon® SF800Z Polycarbonate, 5% Glass Filled
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 10% Glass Filled

Material Notes:
  • MVR (300 °C/1.2 kg) 8.0 cm3/10 min
  • Structural foam
  • 5 % Glass fiber reinforced
  • Milled fiber
  • Chlorine- and bromine-free flame retardant
  • Medium viscosity
  • Easy release
  • Injection molding
  • Available in natural (opaque) and opaque colors
  • In combination with an appropriate blowing agent for the production of structural foam moldings

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.23 g/ccISO 1183
Water Absorption 0.30 %Similar to ISO 62
Moisture Absorption at Equilibrium 0.10 %Similar to ISO 62
Linear Mold Shrinkage, Flow 0.0070 cm/cmISO 294-4,2577
Linear Mold Shrinkage, Transverse 0.0060 cm/cmISO 294-4,2577
Melt Flow 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
estimated from MVR using room temperature density; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 50.0 MPaISO 527-1/-2
Elongation at Break 50 %ISO 527-1/-2
Tensile Modulus 2700 MPaISO 527-1/-2
Impact 4400Puncture - maximum force (N); ISO 6603-2
 5100
@Temperature -30.0 °C
Puncture - maximum force (N); ISO 6603-2
Puncture Energy 35.0 JISO 6603-2
 30.0 J
@Temperature -30.0 °C
ISO 6603-2
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmIEC 60093
Dielectric Constant 3.0
@Frequency 1e+6 Hz
IEC 60250
 3.1
@Frequency 100 Hz
IEC 60250
Dielectric Strength 32.0 kV/mmIEC 60243-1
Dissipation Factor 0.00080
@Frequency 100 Hz
IEC 60250
 0.0090
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 200 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 55.0 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 65.0 µm/m-°CISO 11359-1/-2
Deflection Temperature at 0.46 MPa (66 psi) 138 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 128 °CISO 75-1/-2
Vicat Softening Point 142 °C50°C/h 50N; ISO 306
Flammability, UL94 V-0
@Thickness 3.00 mm
IEC 60695-11-10
Oxygen Index 32 %ISO 4589-1/-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 300 °CInjection Molding; ISO 294
Mold Temperature 110 °CInjection Molding; ISO 10724
Injection Velocity 200 mm/secISO 294
 
Descriptive Properties
AvailabilityEurope
 Near East/Africa
 South and Central America
FeatureRelease agent
FormPellets
ProcessInjection Molding
UL recognitionUL\lh\n

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Bayblend® FR 3021 Polycarbonate + ABS, Mineral Filled
Covestro Bayblend® FR 3020 Polycarbonate + ABS, Mineral Filled
Covestro Bayblend® T90 MF-20 Polycarbonate + ABS, Mineral Filled
Covestro Makrolon® SF805 Polycarbonate, 5% Glass Filled
Covestro Bayblend® T88 GF-20 Polycarbonate + SAN Glass Filled Impact Grade

PB09971 / 92811

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.