MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Brush Wellman Beryllium Copper Alloy 3 Strip; HTR Temper (UNS C17510)  (discontinued **)
Categories: Metal; Nonferrous Metal; Beryllium Alloy; Copper Alloy

Material Notes: Treatment required for max strength: Mill Hardened
Stress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 96%
Stress Relaxation after 1000 hrs @ 200°C: 75%
Formability Ratio, 90° Bend, Radius/Thickness (Good Way): 2.8
Formability Ratio (bad Way): 3.5
Superficial Hardness: 30T 80-84

Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.

Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.

Key Words: ASTM B-534, RWMA Class 3
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.83 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 98 - 103
Hardness, Vickers 216 - 287
Tensile Strength, Ultimate 820 - 1040 MPa
Tensile Strength, Yield 750 - 970 MPa
Elongation at Break 1.0 - 5.0 %
Modulus of Elasticity 138 GPa
Fatigue Strength 300 - 330 MPa
@# of Cycles 1.00e+8
Reverse Bending (R=1)
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000290 - 0.00000360 ohm-cm48-60% IACS Conductivity
 
Thermal PropertiesOriginal ValueComments
CTE, linear 18.0 µm/m-°C
@Temperature 20.0 - 200 °C
Thermal Conductivity 240 W/m-K
Melting Point 1040 - 1080 °C
Solidus 1040 °C
Liquidus 1080 °C
 
Component Elements PropertiesOriginal ValueComments
Beryllium, Be 0.20 - 0.60 %
Copper, Cu 98 %as balance
Nickel, Ni 1.4 - 2.2 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Materion BrushForm® 158 Copper-Nickel-Tin Mill Hardened Strip (UNS C72900), TM00
Materion Beryllium Copper Alloy 3 Rod and Bar; AT (TF00) Temper; All Sizes (UNS C17510)
Materion Beryllium Copper Alloy 3 Strip; AT (TF00) Temper (UNS C17510)
Brush Wellman Beryllium Copper Alloy 3 Strip; A-Planished (TB00) Temper (UNS C17510)
Brush Wellman Beryllium Copper Alloy 3 Strip; A-Dead Soft (TB00) Temper (UNS C17510)

NBB678 / 15277

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.