MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Huntsman PE1501 EVA Film Extrusion  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Film Grade

Material Notes: 5% Vinyl Acetate EVA copolymer and FDA compliant

Features: Yields film with excellent impact strength, good heat seal, and good clarity.

Applications: Film extrusion: greenhouse film, heavy-duty packaging, and ice bags.

FDA Notes: Conforms to FDA regulation 21 CFR 177.1350 under condition of use C through G described in Table 2 of 21 CFR 176.170

Film properties based on 1.0 guage (25 µm) thickness; blow-up ratio 2:1.

Information provided by Huntsman Corporation

Key Words: Poly(Ethylene Vinyl Acetate)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.927 g/cc0.0335 lb/in³ASTM D1505
Thickness 25.4 microns1.00 mil
Melt Flow 0.50 g/10 min0.50 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4747ASTM D2240
Tensile Strength, Ultimate 17.0 MPa2470 psiASTM D638
Tensile Strength, Yield 9.00 MPa1310 psiASTM D638
Film Elongation at Break, MD 400 %400 %ASTM D882
Film Elongation at Break, TD 500 %500 %ASTM D882
Elongation at Break 750 %750 %ASTM D638
Modulus of Elasticity 0.207 GPa30.0 ksiSecant; ASTM D638
Secant Modulus, MD 0.117 GPa17.0 ksiASTM D882
Secant Modulus, TD 0.138 GPa20.0 ksiASTM D882
Dart Drop 11.0 g/micron280 g/milASTM D1709
Dart Drop Test 280 g0.617 lbASTM D1709
Film Tensile Strength at Break, MD 24.0 MPa3480 psiASTM D882
Film Tensile Strength at Break, TD 25.0 MPa3630 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 87.0 °C189 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 6.5 %6.5 %ASTM D1003
Gloss 63 %63 %at 45°; ASTM D523
 
Processing PropertiesMetricEnglishComments
Melt Temperature 204 - 215 °C399 - 419 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHUP12 / 47821

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.