MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Trinseo EMERGE™ PC/ABS 7590 PC/ABS, Flame Retardant
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: Product Description: EMERGE™ PC/ABS 7590 advanced resin is an ignition-resistant PC/ABS blends that contains no chlorinated or brominated flame retardants. Its superior processing makes it ideal for molding large parts and optimizing cycle time productivity in injection molding operations. It has a UL 94 flammability rating of V-0 a 1.5 mm. This resin is suitable for use in a wide variety of applications in the information technology equipment and consumer electronics (ITE/CE) markets.
Main Characteristics: UL 94 V-0 at 1.5 mm; Does not contain chlorine or bromine additives
Applications: TV, monitor and PC enclosures; Adaptors and chargers

Availability: Asia Pacific; North America

Features: Bromine Free; Chlorine Free; Flame Retardant; High Flow; Ignition Resistant

Uses: Electrical Housing; Electrical/Electronic Applications; Housings

Form: Pellets

Processing Method: Injection Molding

Information provided by Trinseo

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cmASTM D955
Melt Flow 17 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D1238
 75 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 6700 psi2.0 in/min; ASTM D638
Tensile Strength, Yield 9000 psi2.0 in/min; ASTM D638
Elongation at Break 50 %2.0 in/min; ASTM D638
Elongation at Yield 4.0 %2.0 in/min; ASTM D638
Flexural Strength 14200 psiASTM D790
Flexural Modulus 410000 psiASTM D790
Izod Impact, Notched 12.0 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 201 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 180 °FUnannealed; ASTM D648
Vicat Softening Point 227 °FRate B (120°C/h), Loading 1 (10 N); ASTM D1525
Flammability, UL94 V-0
@Thickness 1.52 mm
Oxygen Index 29 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Melt Temperature 428 - 482 °F
Mold Temperature 140 - 194 °F
Drying Temperature 176 - 194 °F
Dry Time 3.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTRINSE1531 / 312224

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.