MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Huntsman AVALON® 60 ABX Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Introduction: AVALON 60 ABX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 60 ABX is part of the AVALON Perform Range and offers a specially designed, flexible material with improved slip resistance and rubber-like properties, particularly suitable for TPU/PU applications. The features offered include:
  • Improved processing
  • Lower density
  • Excellent surface definition
  • Abrasion resistance
  • Flex resistance
  • Phthalate free TPU

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³DIN 53479
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6060DIN 53505
Tensile Strength at Break >= 15.0 MPa>= 2180 psiDIN 53504
Elongation at Break >= 600 %>= 600 %DIN 53504
Tear Strength >= 20.0 kN/m>= 114 pliDIN 53515
Abrasion <= 90<= 90mm3; DIN 53516
 
Processing PropertiesMetricEnglishComments
Feed Temperature 25.0 - 35.0 °C77.0 - 95.0 °F
Rear Barrel Temperature 150 - 170 °C302 - 338 °F
Middle Barrel Temperature 155 - 175 °C311 - 347 °F
Front Barrel Temperature 155 - 180 °C311 - 356 °F
Nozzle Temperature 150 - 175 °C302 - 347 °F
Mold Temperature 25.0 - 50.0 °C77.0 - 122 °F
Injection Pressure 2.00 - 10.0 MPa290 - 1450 psi
Hold Pressure 1.00 - 5.00 MPa145 - 725 psi
Back Pressure 0.0300 - 0.300 MPa4.35 - 43.5 psi
Screw Speed 20 - 80 rpm20 - 80 rpm
 
Descriptive Properties
Compression Ratio2-3:1
Flex Life>100 k cyclesDIN 53522 T3
L/D Ratio20-25:1
Typical Screw Diameter40-120 nm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BCC Products BC 8860 Polyurethane Elastomer
BCC Products BC 9020 Silicone RTV Rubber
Huntsman AVALON® 60 AE-ESD Thermoplastic Polyurethane
BASF Elastollan® B 60 A WHA TPUR
Multibase TPSiV® 3040-60A Thermoplastic Silicone Vulcanizate

PHUQ134 / 159507

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.