MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Michelman® GlossCoat™ 100 BL Preprint varnish
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Water based, nonskid preprint varnish for porous substrates

Usage: GlossCoat™ 100BL is a fully formulated, flexo appliable nonskid coating designed for kraft, mottled and bleached substrates.

Application data: GlossCoat™ 100BL should be applied by flexo.

Typical uses include: Beer and beverage containers; POP displays; and Retail packaging

Food Contact Information when manufactured in the USA:
FDA:
176.170: Components of paper and paperboard in contact with aqueous and fatty foods(Restricted).
176.180: Components of paper and paperboard in contact with dry foods.

Food Contact Information when manufactured in Belgium:
FDA:
175.105: Components of adhesives
176.170: Components of paper and paperboard in contact with aqueous and fatty foods(Restricted).
176.180: Components of paper and paperboard in contact with dry foods

When manufactured in Belgium product meets food contact regulations for:
Europe: Euro. Res. AP(2004)1(Restricted)
Germany: BfR Recommendation XIV (Restricted) and BfR Recommendation XXXVI (Restricted)

Information provided by Michelman®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.01 - 1.03 g/cc1.01 - 1.03 g/cc
pH 8.7 - 9.78.7 - 9.7
Brookfield Viscosity 100 - 300 cP100 - 300 cPSpindle # 2, rpm 60
Viscosity Measurement 20 - 2820 - 28[sec], EZ cup, Cup # 2
 
Descriptive Properties
AppearanceOff-white liquid
Solids TypeAcrylic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WMICHEL021 / 134938

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.