Product Description: QSil 573 is a 100% silicone solids elastomer designed for electronic potting applications. The two-component system offers a hard, thermally conductive, low modulus material that is readily repairable. Key Features: - 100% solids
- Excellent thermal conductivity
Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017 |