MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Kraton® G1657 V Linear Triblock Copolymer
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: Kraton G1657 V is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 13%. It is supplied from Taiwan. Kraton G1657 V is used as a modifier of bitumen or thermoplastics and in compound formulations. It may also find use as an ingredient in formulating adhesives, sealants and coatings.

Kraton G1657 VS - is supplied as a dusted, dense pellet.

Information provided by Kraton Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.900 g/cc0.900 g/ccASTM D4025
Viscosity Measure 1200 - 1800 cSt1200 - 1800 cStToluene, 20.0%w; AGAM 922
Melt Index of Compound 22 g/10 min
@Load 5.00 kg,
Temperature 230 °C
22 g/10 min
@Load 11.0 lb,
Temperature 446 °F
Ash 0.020 - 0.12 %0.020 - 0.12 %G1657 VS, silica dusted; AGAM 908
 
Chemical PropertiesMetricEnglishComments
Diblock Content 30 %30 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 47
@Time 10.0 sec
47
@Time 0.00278 hour
Compression molded at 300°F; ASTM D2240
Tensile Strength 23.4 MPa3400 psiCast Film; ASTM D412
Elongation at Break 750 %750 %Cast Film; ASTM D412
300% Modulus 2.41 MPa
@Strain 300 %
350 psi
@Strain 300 %
Cast Film; ASTM D412
 
Descriptive Properties
Antioxidant0.03 to 0.1Test Method KM 08. Non-staining phenolic antioxidant.
Extract in Methanol25
Polystyrene Content (%m)12.3 to 14.3Test Method KM 03. Before hydrogenation.
Styrene / Rubber Ratio13/87
Total Extractables<= 1.5 %mTest Method KM 05
Volatile Matter (%m)<= 1KM 04

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKQZ9026 / 239890

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.