MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Chemours Teflon™ 856G-410 High Build FEP Industrial Coating System
Categories: Polymer; Thermoplastic; Fluoropolymer; Fluorinated Ethylene Propylene (FEP)

Material Notes: Teflon™ fluorinated ethylene propylene (FEP) industrial coatings melt and flow during baking to provide nonporous films. With a maximum operating temperature of 200 °C (400 °F), these industrial coatings have excellent nonstick properties and a low coefficient of friction. In addition to providing excellent chemical resistance, they also have high dielectric strength. These multi-coat systems—commonly used in applications such as mold release that require nonstick properties—are available in water-based liquid and powder form. For some surfaces, it's recommended to use a primer before applying Teflon™ FEP coatings.

Information provided by Chemours.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption <= 0.010 %
@Time 86400 sec
<= 0.010 %
@Time 24.0 hour
ASTM D570
Thickness 25.4 - 50.8 microns1.00 - 2.00 milFilm Build per coat
 <= 178 microns<= 7.00 milMax Total Film Build
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 204 °C399 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 371 °C700 °FCure Temperature
 
Compliance PropertiesMetricEnglishComments
FDA YesYesFood Contact per 21CFR.
 
Descriptive Properties
CarrierWater
Chemical/Solvent ResistanceExcellentASTM D543
ColorClear
Detergent Resistance (hours)480On grit blasted aluminum
 600On aluminum
 744
Salt Spray Resistance Coatings (hours)744+ASTM B117. 5% NaCl at 35 °C (95 °F).
Weather Resistance (years unaffected)20Florida Exposure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDU8712 / 268638

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.