MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ineos N12N-00 Polypropylene Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Grade N12N-00 is a nucleated polypropylene impact copolymer with an excellent balance of stiffness and impact resistance for injection molding applications and compounding products used in Lawn and Garden applications. It has good stiffness and excellent impact resistance even at sub ambient temperature. This meets the requirements of U.S. Food and Drug Administration as specified in 21 CFR 177.1520.
    Applications:
  • General purpose injection molding
  • Compounding
  • Lawn and Garden applications
  • Consumer products
    Benefits:
  • Excellent impact to stiffness balance
  • Low temperature impact resistance

Information provided by Ineos Olefins & Polymers USA

Key Words: Excellent balance of stiffness and impact resistance
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.899 g/ccASTM D792
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 70ASTM D785
Tensile Strength at Break 2570 psi2.0 in/min; ASTM D638
Tensile Strength, Yield 3400 psi2.0 in/min; ASTM D638
Elongation at Break 320 %2.0 in/min; ASTM D638
Elongation at Yield 7.1 %2.0 in/min; ASTM D638
Tensile Modulus 191000 psiASTM D638
Flexural Modulus, 1% Secant 153000 psiASTM D790A
Izod Impact, Notched 1.50 ft-lb/in
@Temperature -20.0 °C
ASTM D256
Izod Impact, Notched (ISO) 3.85 ft-lb/in²
@Temperature -20.0 °C
Area; ASTM D256
 NB
@Temperature 22.8 °C
Area; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 200 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 127 °FUnannealed; ASTM D648
Vicat Softening Point 289 °FASTM D1525
 
Optical PropertiesOriginal ValueComments
Gloss 64 %60°; ASTM D2457
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
ProcessInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ineos H12G-01 Polypropylene Homopolymer
Ineos H36G-01 Polypropylene Homopolymer
Ineos H38G-02 Polypropylene Homopolymer
Ineos R35C-02 Polypropylene Random Copolymer
Phillips Sumika Marlex® ALN-120 Polypropylene Impact Copolymer, Structural foam resin

PINEOS915 / 130374

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.