MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Bamberger Polymers Bapolene® 3042U Polyethylene, Rotational Molding Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Bapolene 3042U is a hexene linear low density polyethylene designed to provide an excellent combination of ESCR and impact. It contains a UV additive package and complies with US FDA 21CFR177.1520.

Applications: Containers; Drums; Industrial Tanks.

All data is based on molded plaques.

Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers

Key Words: Food Contact Acceptable; Hexene Comonomer; High ESCR (Stress Crack Resistance); High Impact Resistance; UV Resistant
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.936 g/cc0.0338 lb/in³ASTM D-1505
ESCR 100% Igepal® >= 1000 hour>= 1000 hourASTM D-1693
Melt Flow 5.0 g/10 min5.0 g/10 minASTM D-1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 17.9 MPa2600 psiASTM D-638
Flexural Modulus 0.596 GPa86.5 ksiASTM D-790
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
processRotational Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade
Bamberger Polymers Bapolene® 3039U Polyethylene, Rotational Molding Grade
Braskem ML3601U LLDPE Rotomolding Polyethylene
LyondellBasell Lupolen 3621 M RM Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade
Overview of materials for Linear Medium Density Polyethylene (LMDPE), Rotational Molded

PBP3B160 / 20808

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.