MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

Superior Flux Superior 8600 Water-Soluble RMA Tacky Flux
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes:
  • Residues are completely Water-Soluble and the flux’s characteristics pass Bellcore.
  • Will solder a wide range of difficult-to-solder base metals
  • Halide-free, halogen-free
  • Superior wetting characteristics, lot-to-lot consistency, and stable viscosity
  • Translucent residue
  • Long tack time
  • No slump
Description: Superior 8600 RMA Water-Soluble RMA Tacky Flux is a Water-Soluble formulation for electronics applications requiring high-reliability, stability, and cleanliness. Flux formulation contains no ionic materials and is suitable for clean-room applications.

Applications: Superior 8600 RMA Water-Soluble RMA Tacky Flux is formulated for BGA rework and repair, or specialty processes where a conventional flux does not provide sufficient activity and/or requires post-solder cleaning. Flux can be placed on surface area by printing, dispensing, or manually applying the flux. When cleaning all residues, a water temperature of 60ºC/140ºF is recommended for optimum results. Residues are watersoluble.

Information provided by Superior Flux

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 100500 - 109500 cP100500 - 109500 cP
 
Thermal PropertiesMetricEnglishComments
Melting Point 60.0 °C140 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 120 - 400 °C248 - 752 °FSoldering Range
Shelf Life 1.00 Month1.00 Month
 
Descriptive Properties
ColorAmber
FormPaste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NSFLUX098 / 185782

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.