MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Geon® Performance Solutions CPVC MC200 Chlorinated Polyvinyl Chloride (CPVC)  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); Chlorinated PVC (CPVC)

Material Notes: Geon MC200 CPVC is an Injection molding fitting compound. It is listed under NSF Std 14 and 61 and meets or exceeds ASTM D-1784 Cell Class 23447. MC200 is designed for IPS applications where enhanced resistance at elevated temperatures is needed. MC200 demonstrates ease of processing with excellent thermal stability.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.48 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 117ASTM D785
Hardness, Shore D 84ASTM D2240
Tensile Strength, Yield 54.5 MPaType I, 5.1 mm/min; ASTM D638
Tensile Modulus 2900 MPaType I, 5.1 mm/min; ASTM D638
Flexural Strength 93.1 MPaASTM D790
Flexural Modulus 2760 MPaASTM D790
Izod Impact, Notched 160 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 105 °C
@Thickness 3.18 mm
Annealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 199 - 207 °C
 
Descriptive Properties
Agency RatingsNSF 14
 NSF 61
FormsPellets
Generic NamePolyvinyl Chloride, Chlorinated (CPVC)
Processing MethodInjection Molding
PVC Cell Classification23447ASTM D1784
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesFittings

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Geon® Performance Solutions CPVC MC100 Polyvinyl Chloride, Chlorinated (CPVC)
Geon® Performance Solutions CPVC EC950 Polyvinyl Chloride, Chlorinated (CPVC)
Geon® Performance Solutions CPVC MC250 Polyvinyl Chloride, Chlorinated (CPVC)
Geon® Performance Solutions CPVC MC500 Polyvinyl Chloride, Chlorinated (CPVC)
Vycom FLAMETEC™ CPVC Chlorinated Polyvinyl Chloride Sheet

PH1PN8167 / 102003

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.