MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Sandvik 21-6-9 AEROSPACE Tube and Pipe, Seamless
Categories: Metal; Ferrous Metal; Austenitic

Material Notes: Sandvik 21-6-9 is an austenitic grade with a high level of Mn, a low level of Ni and the addition of N. The grade is characterized by:
  • High mechanical strength in the hard condition
  • Very good impact toughness in temperatures down to -230°C (-382°F)
  • Very good high temperature oxidation resistance
Applications: Sandvik 21-6-9 seamless tube is used for components in the aircraft industry as well as in medical and cryogenic applications.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.81 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate >= 655 MPaRm, annealed
Tensile Strength, Yield >= 330 MPa
@Strain 0.2 %
annealed
Elongation at Break >= 35 %annealed
Modulus of Elasticity 200 GPa
Poissons Ratio 0.285
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.480 J/g-°C
@Temperature 0.000 °C
 0.480 J/g-°C
@Temperature 100 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.040 %
Chromium, Cr 19 - 21.5 %
Copper, Cu <= 0.75 %
Manganese, Mn 8.0 - 10 %
Molybdenum, Mo <= 0.75 %
Nickel, Ni 5.5 - 7.5 %
Nitrogen, N 0.15 - 0.40 %
Phosphorus, P <= 0.030 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
202 Stainless Steel, Annealed Bar
Sandvik 21-6-9 AEROSPACE Tubing, Welded an Redrawn
202 Stainless Steel, 1/4 Hard Sheet, Strip
Lucas-Milhaupt Silvaloy® 852 Silver Based Cadmium Free Filler Metal
Lucas-Milhaupt HANDY HI-TEMP 870 High Temperature Alloy

NSANDV5284 / 199848

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.