MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Permabond 265 Cyanoacrylate
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: PERMABOND 265 is a medium viscosity cyanoacrylate ideal for intermediate gap fill application. PERMABOND 265 provides faster set times and improved gap-filling capability compared to conventional cyanoacrylates. The adhesive bonds to a wide range of substrates including metals, ceramics, plastics and elastomers. It is excellent for bonding difficult-to-bond plastics such as polyacetals.

Features and Benefits:

  • Instant Setting
  • Improved Gap Filling
  • Faster Strength Development
  • Improved Bonding to Difficult Surfaces
  • High Shear Strength
  • Easy to Apply
  • One Part System

Soluble in Nitroethane, Methyl Ethyl Ketone, Acetone

Information provided by Permabond.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/ccUncured
Viscosity 400 cP
@Temperature 25.0 °C
Uncured
Storage Temperature 2.00 - 7.00 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 85
Adhesive Bond Strength 8.30 MPaAluminum, Shear
 20.0 MPaGrit blasted steel, Shear
Impact 6.3 - 14.7kJ/m2 Adhesive Impact Strength; ASTM D950
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 9.84 kV/mm
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 82.0 °C
Minimum Service Temperature, Air -60.0 °C
Flash Point 83.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 10.0 secSteel, set time
 10.0 secBuna N Rubber, set time
 10.0 secPhenolic, set time
 24.0 hour
@Temperature 25.0 °C
full strength
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceColorlessUncured
Maximum Gap Fill (mm)0.2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPERMA861 / 162755

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.