MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

MetalTek J92240 14-4 PH® Precipitation Hardening Steel
Categories: Metal; Ferrous Metal; Stainless Steel; Cast Stainless Steel; Precipitation Hardening Stainless

Material Notes: Produced under license of ARMCO Advanced Materials Corp.

Information provided by MetalTek

Key Words: Cast UNS J92240; Cast Grade 14-4PH; Cast ASTM ; AMS 5340
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 286286
Tensile Strength, Ultimate >= 1030 MPa>= 149000 psi
Tensile Strength, Yield >= 895 MPa>= 130000 psi
Elongation at Break >= 10 %>= 10 %
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.060 %<= 0.060 %
Chromium, Cr 13.5 - 14.25 %13.5 - 14.25 %
Copper, Cu 3.0 - 3.5 %3.0 - 3.5 %
Iron, Fe 72.79 - 77.1 %72.79 - 77.1 %As Balance
Manganese, Mn <= 0.70 %<= 0.70 %
Molybdenum, Mo 2.0 - 2.5 %2.0 - 2.5 %
Nickel, Ni 3.75 - 4.75 %3.75 - 4.75 %
Niobium, Nb (Columbium, Cb) 0.15 - 0.35 %0.15 - 0.35 %
Nitrogen, N <= 0.050 %<= 0.050 %
Silicon, Si 0.50 - 1.0 %0.50 - 1.0 %
Tantalum, Ta <= 0.050 %<= 0.050 %
 
Descriptive Properties
Heat TreatmentHomog, Solution, Age

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
17-7 PH Stainless Steel, CH900, plate, sheet, and strip
AISI Type S13800 Stainless Steel (PH 13-8 Mo) longitudinal properties, condition RH950
Cast Stainless Steel CB7Cu-1, ASTM A747
Cast Stainless Steel CB7Cu-2, ASTM A747
Cast Stainless Steel CH20, ASTM A351

NMETEK067 / 18317

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.