MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Sandvik 25.20.C Welding wire
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Sandvik 25.20.C is a filler material suitable for joining heat resistant austenitic steels of the 25 Cr/20 Ni type. It can be used in air up to about 1100°C (2010°F), in oxidizing sulphurous atmospheres up to 1050°C (1920°F) and in reducing sulphurous atmospheres up to 650°C (1200°F). Sandvik 25.20.C has moderate creep strength and structure stability.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 160160
Tensile Strength, Ultimate  490 MPa
@Temperature 400 °C
71100 psi
@Temperature 752 °F
 590 MPa
@Temperature 20.0 °C
85600 psi
@Temperature 68.0 °F
Tensile Strength, Yield  250 MPa
@Strain 0.2 %,
Temperature 400 °C
36300 psi
@Strain 0.2 %,
Temperature 752 °F
 390 MPa
@Strain 0.2 %,
Temperature 20.0 °C
56600 psi
@Strain 0.2 %,
Temperature 68.0 °F
Elongation at Break  26 %
@Temperature 400 °C
26 %
@Temperature 752 °F
 38 %
@Temperature 20.0 °C
38 %
@Temperature 68.0 °F
Reduction of Area 64 %64 %
Charpy Impact  60.0 J
@Temperature -196 °C
44.3 ft-lb
@Temperature -321 °F
 130 J
@Temperature 20.0 °C
95.9 ft-lb
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 19.7 µm/m-°C
@Temperature 20.0 - 400 °C
10.9 µin/in-°F
@Temperature 68.0 - 752 °F
Thermal Conductivity  12.0 W/m-K
@Temperature 20.0 °C
83.3 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 13.0 W/m-K
@Temperature 100 °C
90.2 BTU-in/hr-ft²-°F
@Temperature 212 °F
 15.0 W/m-K
@Temperature 300 °C
104 BTU-in/hr-ft²-°F
@Temperature 572 °F
 17.0 W/m-K
@Temperature 500 °C
118 BTU-in/hr-ft²-°F
@Temperature 932 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.10 %0.10 %All-weld metal
 0.12 %0.12 %AIM
Chromium, Cr 25 %25 %All-weld metal
 26 %26 %AIM
Copper, Cu <= 0.30 %<= 0.30 %AIM
Manganese, Mn 1.7 %1.7 %All-weld metal
 1.8 %1.8 %AIM
Molybdenum, Mo <= 0.30 %<= 0.30 %AIM
Nickel, Ni 20 %20 %All-weld metal
 21 %21 %AIM
Nitrogen, N 0.050 %0.050 %All-weld metal
 <= 0.060 %<= 0.060 %AIM
Phosphorus, P 0.012 %0.012 %All-weld metal
 <= 0.015 %<= 0.015 %AIM
Silicon, Si 0.30 %0.30 %AIM
 0.30 %0.30 %All-weld metal
Sulfur, S 0.010 %0.010 %All-weld metal
 <= 0.015 %<= 0.015 %AIM

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NSANDV5136 / 199700

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.