MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Magnesium HK31A-T6, Sheet
Categories: Metal; Nonferrous Metal; Magnesium Alloy

Key Words: UNS M13310
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 55500 kg load, 10 mm ball (Cast)
Tensile Strength, Ultimate 255 MPa
@Temperature 20.0 °C
 55.0 MPa
@Temperature 315 °C,
Time 3.60e+6 sec
tested at elevated temperature
 115 MPa
@Temperature 315 °C,
Time 601 sec
tested at elevated temperature
 180 MPa
@Temperature 150 °C,
Time 601 sec
Creep Strength 17.0 MPa
@Temperature 315 °C,
Time 360000 sec
0.2% total extension
 69.0 MPa
@Temperature 205 °C,
Time 360000 sec
0.2% total extension
Modulus of Elasticity 25.0 GPa
@Temperature 315 °C
 40.0 GPa
@Temperature 205 °C
Tensile Modulus 45.0 GPa
Poissons Ratio 0.35
Machinability 100 %Relative Rating, 100=Best (Cast)
Shear Modulus 17.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000770 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 325 J/g
CTE, linear 26.8 µm/m-°C
@Temperature 0.000 - 100 °C
 27.0 µm/m-°C
@Temperature 20.0 - 200 °C
Estimated from similar Mg alloys
Specific Heat Capacity 1.00 J/g-°C
Thermal Conductivity 92.0 W/m-K
Melting Point 590 - 650 °C
Solidus 590 °C
Liquidus 650 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu <= 0.10 %
Magnesium, Mg 96 %As Remainder
Nickel, Ni <= 0.010 %
Thorium, Th 2.5 - 4.0 %
Zinc, Zn <= 0.30 %
Zirconium, Zr 0.40 - 1.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Magnesium AZ31B-O, Annealed Sheet
Magnesium, Mg; Annealed Sheet
Magnesium HM21A-T8, Sheet and Plate
Magnesium, Mg; Hard-Rolled Sheet
Magnesium HK31A-O, Plate

MMHK31c / 147534

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.