MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Epoxies, Etc 40-3901 Electrically Conductive Epoxy Adhesive
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: 40-3901 is a two component epoxy adhesive filled with silver. This electrically conductive epoxy resin formulation offers an easy one to one mix ratio that cures at room temperature. 40-3901 is designed for adhesive bonding in microelectronic and optoelectronic applications. Due to its excellent continuity of conductivity, it has also been used extensively in applications such as micro-wave EMI and RFI shielding, in the assembly or repair of printed circuit boards, wave guides, electronic modules, flat cable, high frequency shields, connectors, circuitry, and as a cold solder. 40-3901 is formulated with pure silver (no alloys). Both the resin and hardener have silver particles dispersed.

Features:

  • Electrically conductive
  • Thermally conductive
  • Room temperature cure
  • Easy 1:1 mix ratio
  • Good bond strength

Information provided by Epoxies, Etc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.80 g/cc1.80 g/ccHardener
 3.10 g/cc3.10 g/ccResin
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7070
Flexural Strength 70.3 MPa10200 psi
Shear Strength 4.83 MPa700 psiLapshear (Al to Al)
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.0060 ohm-cm0.0060 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 7.93 W/m-K55.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 135 °C275 °F
Minimum Service Temperature, Air -35.0 °C-31.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  15.0 min
@Temperature 90.0 °C
0.250 hour
@Temperature 194 °F
 60.0 min
@Temperature 65.0 °C
1.00 hour
@Temperature 149 °F
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Shelf Life 12.0 Month
@Temperature 25.0 °C
12.0 Month
@Temperature 77.0 °F
 
Descriptive Properties
ColorSilver
Mix Ratio1:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFEPOX093 / 316770

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.