MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Meehanite Almanite® WS Wear and Abrasion Resisting Cast Iron
Categories: Metal; Ferrous Metal; Cast Iron; White Cast Iron; Martensitic

Material Notes: Type WS is a hard wearing martensitic iron with exceptional impact strength...not readily machinable...work hardens in service to high hardness values. Type WS is recommended for crusher jaws, impact hammers, pulverizers, etc.

General Meehanite information - Meehanite metal is first melted to a definite degree of undercooling or constitution which is related to the section of the casting to be poured and the range of physical properties such as tensile strength and hardness required. Nucleation with patented mixtures of graphitizing agents results in the removal of undercooling, in the controlled precipitation of graphite and in a fine grained eutectic cell structure which determines the density and physical integrity of the casting. Ordinary cast irons made to chemical specifications which do not include the benefit of controlled undercooling are influenced by mass effect to a maximum degree and for this and other reasons cannot be considered an equivalent to Meehanite metal.

Information provided by Meehanite Marketing Association.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.65 - 7.75 g/cc0.276 - 0.280 lb/in³Typical value of white cast iron
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 400 - 525400 - 525Nominal
Tensile Strength, Ultimate 414 - 552 MPa60000 - 80000 psi
Tensile Strength, Yield 345 - 448 MPa50000 - 65000 psi
Elongation at Break 2.0 - 4.0 %2.0 - 4.0 %
Modulus of Elasticity 165 GPa24000 ksi
Izod Impact Unnotched <= 244 J
@Diameter 30.5 mm
<= 180 ft-lb
@Diameter 1.20 in
bar

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Meehanite Almanite® WSH Wear and Abrasion Resisting Cast Iron
Meehanite Almanite® W1 Wear and Abrasion Resisting Cast Iron
AISI 4024 Steel
Class III Type E 25% Cr Martensitic White Cast Iron
Meehanite Almanite® W4 Wear and Abrasion Resisting Cast Iron

NMEE16 / 18237

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.