MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Pressure Seal 3726 Nitrile - Butadiene
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Compound 3726 is a 70 durometer gray colored Buna N elastomer, it is formulated with FDA approved materials.

This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 2 BF 715 EO14 EO34; 2 BG 715 EO14 EO34 EA14 EF11; 5 BG 712 A14 EO14 EO34
This Compound is RoHS Compliant

Information provided by Pressure Seals Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.49 g/cc1.49 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7272
 54
@Treatment Temp. 23.0 °C,
Time 252000 sec
54
@Treatment Temp. 73.4 °F,
Time 70.0 hour
ASTM Reference Fuel B
 69
@Treatment Temp. 100 °C,
Time 252000 sec
69
@Treatment Temp. 212 °F,
Time 70.0 hour
Distilled water aged
 70
@Treatment Temp. 23.0 °C,
Time 252000 sec
70
@Treatment Temp. 73.4 °F,
Time 70.0 hour
ASTM Reference Fuel A
 70
@Treatment Temp. 100 °C,
Time 252000 sec
70
@Treatment Temp. 212 °F,
Time 70.0 hour
ASTM Oil #3
 70
@Treatment Temp. 125 °C,
Time 252000 sec
70
@Treatment Temp. 257 °F,
Time 70.0 hour
Heat Aged, Test Tube Method
 71
@Treatment Temp. 100 °C,
Time 252000 sec
71
@Treatment Temp. 212 °F,
Time 70.0 hour
ASTM Oil #1
 73
@Treatment Temp. 100 °C,
Time 252000 sec
73
@Treatment Temp. 212 °F,
Time 70.0 hour
Heat Aged
 73
@Treatment Temp. 125 °C,
Time 252000 sec
73
@Treatment Temp. 257 °F,
Time 70.0 hour
Heat Aged
Tensile Strength 11.18 MPa1622 psi
 9.6844 MPa
@Treatment Temp. 125 °C,
Time 252000 sec
1404.6 psi
@Treatment Temp. 257 °F,
Time 70.0 hour
Heat Aged
 9.6851 MPa
@Treatment Temp. 125 °C,
Time 252000 sec
1404.7 psi
@Treatment Temp. 257 °F,
Time 70.0 hour
Heat Aged, Test Tube Method
 10.533 MPa
@Treatment Temp. 23.0 °C,
Time 252000 sec
1527.7 psi
@Treatment Temp. 73.4 °F,
Time 70.0 hour
ASTM Reference Fuel B
 10.814 MPa
@Treatment Temp. 23.0 °C,
Time 252000 sec
1568.5 psi
@Treatment Temp. 73.4 °F,
Time 70.0 hour
ASTM Reference Fuel A
 11.250 MPa
@Treatment Temp. 100 °C,
Time 252000 sec
1631.7 psi
@Treatment Temp. 212 °F,
Time 70.0 hour
Heat Aged
 11.3510 MPa
@Treatment Temp. 100 °C,
Time 252000 sec
1646.33 psi
@Treatment Temp. 212 °F,
Time 70.0 hour
ASTM Oil #1
 12.917 MPa
@Treatment Temp. 100 °C,
Time 252000 sec
1873.4 psi
@Treatment Temp. 212 °F,
Time 70.0 hour
ASTM Oil #3
Elongation, Ultimate 621 %621 %
 482.5 %
@Treatment Temp. 125 °C,
Time 252000 sec
482.5 %
@Treatment Temp. 257 °F,
Time 70.0 hour
Heat Aged
 482.5 %
@Treatment Temp. 125 °C,
Time 252000 sec
482.5 %
@Treatment Temp. 257 °F,
Time 70.0 hour
Heat Aged, Test Tube Method
 497.4 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
497.4 %
@Treatment Temp. 73.4 °F,
Time 70.0 hour
ASTM Reference Fuel B
 547.1 %
@Treatment Temp. 100 °C,
Time 252000 sec
547.1 %
@Treatment Temp. 212 °F,
Time 70.0 hour
Heat Aged
 573.2 %
@Treatment Temp. 100 °C,
Time 252000 sec
573.2 %
@Treatment Temp. 212 °F,
Time 70.0 hour
ASTM Oil #1
 617.9 %
@Treatment Temp. 100 °C,
Time 252000 sec
617.9 %
@Treatment Temp. 212 °F,
Time 70.0 hour
ASTM Oil #3
 617.9 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
617.9 %
@Treatment Temp. 73.4 °F,
Time 70.0 hour
ASTM Reference Fuel A
100% Modulus 2.14 MPa311 psi
Tear Strength 27.5 kN/m157 pliDie B
 34.9 kN/m199 pliDie C
Compression Set  29.4 %
@Treatment Temp. 100 °C,
Time 79200 sec
29.4 %
@Treatment Temp. 212 °F,
Time 22.0 hour
Solid
 31.5 %
@Treatment Temp. 125 °C,
Time 79200 sec
31.5 %
@Treatment Temp. 257 °F,
Time 22.0 hour
Solid
 33.7 %
@Treatment Temp. 100 °C,
Time 79200 sec
33.7 %
@Treatment Temp. 212 °F,
Time 22.0 hour
Plied
 39 %
@Treatment Temp. 100 °C,
Time 252000 sec
39 %
@Treatment Temp. 212 °F,
Time 70.0 hour
Solid
 39.8 %
@Treatment Temp. 125 °C,
Time 79200 sec
39.8 %
@Treatment Temp. 257 °F,
Time 22.0 hour
Plied
 45.6 %
@Treatment Temp. 100 °C,
Time 252000 sec
45.6 %
@Treatment Temp. 212 °F,
Time 70.0 hour
Plied
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -23.3 °C-10.0 °F
Shrinkage  -3.60 %
@Treatment Temp. 100 °C,
Time 252000 sec
-3.60 %
@Treatment Temp. 212 °F,
Time 70.0 hour
Volume, ASTM Oil #1
 2.9 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
2.9 %
@Treatment Temp. 73.4 °F,
Time 70.0 hour
Volume, ASTM Reference Fuel A
 5.9 %
@Treatment Temp. 100 °C,
Time 252000 sec
5.9 %
@Treatment Temp. 212 °F,
Time 70.0 hour
Volume, Distilled water aged
 7.3 %
@Treatment Temp. 100 °C,
Time 252000 sec
7.3 %
@Treatment Temp. 212 °F,
Time 70.0 hour
Volume, ASTM Oil #3
 31.7 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
31.7 %
@Treatment Temp. 73.4 °F,
Time 70.0 hour
Volume, ASTM Reference Fuel B
 
Descriptive Properties
ColorGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPRESL020 / 318230

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.