MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
A. Schulman Premi-Glas® 1285VE 1285 VE Glass Reinforced Vinyl Ester SMC  (discontinued **)
Categories: Polymer; Thermoset; Composite SMC; Filled/Reinforced Thermoset; Vinyl Ester; Vinyl Ester Sheet Molding Compound

Material Notes: Description: Premi-Glas® 1285 VE is a glass reinforced vinyl ester sheet molding compound designed for automotive under the hood applications.

Key features and benefits:

  • Designed for compression molding for optimal strength on large-span covers
  • Excellent resistance to automotive chemicals and fluids, and to salt spray
  • Replaces cast metals for reduced Noise, Vibration and Harshness, plus molded-in color
  • Meets the requirements of GMP.UP.018
  • Excellent thermal properties and elevated temperature modulus retention

Market: Composite PowerTrain

Information provided by Premix.

A. Schulman has acquired this former Premix product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.80 g/ccASTM D792
Water Absorption 0.20 %ISO 62
Linear Mold Shrinkage 0.00026 cm/cmISO 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 12500 psiISO 62
 8500 psi
@Temperature 150 °C
ISO 62
Tensile Modulus 2.20e+6 psitangent; ISO 527
 1.20e+6 psi
@Temperature 150 °C
ISO 527
Flexural Strength 25500 psiISO 178
 17500 psi
@Temperature 150 °C
ISO 178
Flexural Modulus 900000 psi
@Thickness 2.50 mm,
Temperature 150 °C
Secant; ISO 178
 1.20e+6 psi
@Thickness 2.50 mm,
Temperature 22.0 °C
Secant; ISO 178
 1.20e+6 psi
@Thickness 0.500 mm,
Temperature 150 °C
Secant; ISO 178
 1.70e+6 psi
@Thickness 0.500 mm,
Temperature 22.0 °C
Secant; ISO 178
Izod Impact, Unnotched 24.0 ft-lb/inASTM D4812
Impact 0.23(in) High Speed Impact (Deflection Max Load); ISO 6603-2
 517(lb) High Speed Impact (Impact Max Load); ISO 6603-2
Instrumented Impact Total Energy 9.30 ft-lbHigh Speed Impact (Total Energy); ISO 6603-2
Instrumented Impact Energy at Peak 5.10 ft-lbHigh Speed Impact (Energy Max Load); ISO 6603-2
 
Thermal PropertiesOriginal ValueComments
CTE, linear 15.0 µin/in-°F
@Temperature 20.0 °C
Z-direction; ASTM D696
CTE, linear, Transverse to Flow 10.0 µin/in-°F
@Temperature 20.0 °C
XY-direction; ASTM D696
Thermal Conductivity 3.82 BTU-in/hr-ft²-°FASTM 1530-93
Glass Transition Temp, Tg 370 °FISO 6721 DMS

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman Premi-Glas® 1265 VE 1265-VE (Injection Compression Molded) Glass Reinforced Vinyl Ester TMC
Menzolit Menzolit® BMC 3000 Unsaturated Polyester UP
Haysite 44500 Vinyl Ester SMC, 30% Glass Reinforced
Electrolytic Tough Pitch (ETP) Copper, UNS C11000, OSO25 Temper flat products, tube
Celanese VECTRA C130 LCP, 30% Glass Reinforced

PPREMI11 / 58138

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.