MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lord Adhesives Metech 3233 / 3236 Two Part Conductor System
Categories: Polymer; Thermoset

Material Notes: Two part silver termination system for use on P.T.C. thermistor bodies. 3233 is the ohmic contact bottom coat and 3236 is the solderable silver top coat. These materials are screen printable and are designed to be cofired. When applied properly, the resulting cofired film will provide excellent ohmic contact and be readily solderable.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity 75000 - 110000 cP
@Temperature 25.0 °C
3236 (Top); Spindle #7 @ 20rpm
 90000 - 120000 cP
@Temperature 25.0 °C
3233 (Ohmic); Spindle #7 @ 20rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ashley Polymers Ashlene® P266 PPO, 30% Glass Reinforced
Overview of materials for PPE/PPO + Carbon Fiber
Avient Lubri-Tech™ MP-10GF/10T Modified Polyphenylene Oxide (mPPO), Glass Filled, PTFE Lubricated
A. Schulman ComAlloy Hiloy® 283 PPO Alloy, Glass Reinforced

PLORD059 / 86067

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.