MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Scandium, Sc
Categories: Metal; Nonferrous Metal; Pure Element

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 3.00 g/cc
 
Chemical PropertiesOriginal ValueComments
Atomic Mass 44.9559101995
Atomic Number 21
X-ray Absorption Edge 2.7572 ÅK
 26.831 ÅLI
 30.161 ÅLII
 30.457 ÅLIII
Electronegativity 1.36Pauling
Ionic Radius 0.732 ÅCrystal Ionic Radius for Valence +3
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 36(0101) face
 132(0001) face
Tensile Strength, Ultimate 255 MPa
Tensile Strength, Yield 173 MPa
Elongation at Break 5.0 %
Tensile Modulus 74.4 GPa
Bulk Modulus 56.6 GPa
Poissons Ratio 0.279
Shear Modulus 29.1 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000509 ohm-cm
Magnetic Susceptibility 0.000007006cgs/g
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 350 J/g
CTE, linear 7.60 µm/m-°Calong a-axis
 15.3 µm/m-°Calong c-axis
 10.2 µm/m-°C
@Temperature 20.0 °C
Bulk
Specific Heat Capacity 0.540 J/g-°C
Thermal Conductivity 6.30 W/m-K
Melting Point 1539 °C
Boiling Point 2836 °C
 
Component Elements PropertiesOriginal ValueComments
Scandium, Sc 100 %
 
Descriptive Properties
CAS Number7440-20-2

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 1020 Steel, cold rolled
Overview of materials for High Carbon Steel
Overview of materials for AISI 4000 Series Steel
Copper-Nickel-Phosphorus alloy, UNS C19000
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded

AMESc00 / 100

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.