MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

International Mold Steel NAK80 Precipitation Hardened Mold Steel
Categories: Metal; Ferrous Metal; Tool Steel; Mold Steel

Material Notes: Description: NAK80 is a precipitation or age-hardened mold steel with a uniform through hardness of approximately 40 HRc. It is super clean, Vacuum-Arc Remelted steel with uniform grain structure, uniform hardness, and excellent dimensional stability.

Unique Characteristics:

  • Super clean, Vacuum-Arc Remelt manufacturing process.
  • 40 HRc hardness.
  • Age-hardened for uniformity of hardness throughout, even in heavy sections.
  • When welded, NAK leaves no witness lines after re-aging.
  • Uniform grain structure with no pin holes, inclusions or hard spots.
  • Machines up to 20% faster than 30 HRc P20 mold steels.
  • Never needs stress relieving, even after heavy machining.
  • Polishes to a superior No. 1 finish, even over welded areas.

Applications:

  • Clear lens molds
  • Extremely critical diamond finish applications
  • Molds requiring special EDM finish

Information provided by International Mold Steel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 4040
Tensile Strength, Ultimate 1264 MPa183400 psi
Tensile Strength, Yield 1018 MPa
@Strain 0.2 %
147600 psi
@Strain 0.2 %
Elongation at Break 16.1 %16.1 %Elongation in 2" (longitudinal)
Reduction of Area 41.9 %41.9 %
Modulus of Elasticity 207 GPa
@Temperature 23.0 °C
30000 ksi
@Temperature 73.4 °F
Charpy Impact 11.0 J8.10 ft-lbV-Notch, Longitudinal
 11.5 J8.50 ft-lbV-Notch, Transverse
 
Electrical PropertiesMetricEnglishComments
Magnetic Permeability <= 380<= 380
Magnetic Coercive Force, Hc 14 Oe14 Oe
Magnetic Saturation Flux Density, Bmax 16360 Gauss16360 GaussSaturate Magnetism
Magnetic Remanence, Br 8500 Gauss8500 GaussResidual Magnetism
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.3 µm/m-°C
@Temperature 20.0 - 100 °C
6.30 µin/in-°F
@Temperature 68.0 - 212 °F
 12.6 µm/m-°C
@Temperature 20.0 - 200 °C
7.00 µin/in-°F
@Temperature 68.0 - 392 °F
 13.5 µm/m-°C
@Temperature 20.0 - 300 °C
7.50 µin/in-°F
@Temperature 68.0 - 572 °F
Thermal Conductivity  41.33 W/m-K
@Temperature 93.3 °C
286.8 BTU-in/hr-ft²-°F
@Temperature 200 °F
 42.19 W/m-K
@Temperature 204 °C
292.8 BTU-in/hr-ft²-°F
@Temperature 400 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 1.0 %1.0 %
Carbon, C 0.15 %0.15 %
Copper, Cu 1.0 %1.0 %
Iron, Fe 93.05 %93.05 %
Manganese, Mn 1.5 %1.5 %
Nickel, Ni 3.0 %3.0 %
Silicon, Si 0.30 %0.30 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bohler-Uddeholm UDDEHOLM ORVAR® SUPREME (Premium AISI H13) Hot Work Tool Steel
International Mold Steel NAK55 Precipitation Hardened Mold Steel
Bohler-Uddeholm P20 PREMIUM MODIFIED Pre-hardened Mold Steel
Bohler-Uddeholm COMPAX™ AISI S7 MOLD QUALITY Cold Work Steel
Bohler-Uddeholm UDDEHOLM RAMAX® S Modified 420F

NIMS01 / 17380

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.