MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

LyondellBasell Lupolen 2421D LDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Lupolen 2421 D is Low Density Polyethylene additivated with antioxidant package. It is delivered in pellet form.

Availability: Africa-Middle East; Asia-Pacific; Europe

Application: Agriculture Film; Bags & Pouches; Heavy Duty Packaging; Liner Film; Shrink Film; Stretch Hood

Market: Flexible Packaging

Processing Method: Blown Film

Attribute: General Purpose; Good Processability; Good Tear Strength; Good Toughness

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.923 g/cc0.0333 lb/in³ISO 1183-1
Melt Flow 0.250 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.250 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 10.0 MPa1450 psiISO 527-1, -2
Film Elongation at Break, MD 200 %200 %ISO 527-1, -3
Film Elongation at Break, TD 500 %500 %ISO 527-1, -3
Tensile Modulus 0.260 GPa37.7 ksiISO 527-1, -2
Coefficient of Friction >= 0.800>= 0.800ISO 8295
Dart Drop Test 250 g0.551 lbF50; ASTM D1709
Film Tensile Strength at Break, MD 27.0 MPa3920 psiISO 527-1, -3
Film Tensile Strength at Break, TD 25.0 MPa3630 psiISO 527-1, -3
 
Thermal PropertiesMetricEnglishComments
Melting Point 110 °C230 °FPeak; ISO 11357-3
Vicat Softening Point 96.0 °C205 °FA50; ISO 306
 
Optical PropertiesMetricEnglishComments
Haze <= 14.0 %
@Thickness 0.0500 mm
<= 14.0 %
@Thickness 0.00197 in
ASTM D1003
Gloss >= 15.0 %>= 15.0 %20°; ASTM D2457
 >= 50.0 %>= 50.0 %60°; ASTM D2457
 
Descriptive Properties
Failure Energy6.5 J/mm70 µm, DIN 53373

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQS9651 / 324586

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.