MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik VESTAMID® NRG 2901 PA 12  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, Extrusion/Tubing Grade

Material Notes: VESTAMID® NRG 2901 is a high molecular, heat stabilized compound with exceptional mold release properties. Additionally VESTAMID®NRG 2901 is nucleated to reduce the cycle time and shrinkage of molded parts. Generally mechanical properties of compounds based on PA 12 vary little with changing humidity due to their low moisture absorption. Parts made of this semi-crystalline material are characterized by exceptional impact strength, high abrasion resistance, low friction and good chemical resistance. Manufacturer recommends a processing temperature between 230°C (446°F) and 260°C (500°F) – in some cases up to 280°C (536°F) - during the injection molding process. The mold temperature should be within a range of 60°C (140°F) to 100°C (212°F). Drying at 80°C (176°F) for 2 hours to 4 hours before processing is recommended. Polyamide 12 is a high performance thermo plastic polymer with increased performance characteristics that translates into safe operations over the life of the installed pipeline. It has a considerable record of safe and proven experience in many demanding applications, including fuel lines in passenger cars, air brake tubing in trucks and off-shore applications.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0067 cm/cm0.0067 in/indetermined on 2 mm sheets with film gate at rim mold temperature 180°C; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0115 cm/cm0.0115 in/indetermined on 2 mm sheets with film gate at rim mold temperature 180°C; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 45.0 MPa6530 psiISO 527
Elongation at Break >= 50 %>= 50 %ISO 527
Elongation at Yield 5.0 %5.0 %ISO 527
Tensile Modulus 1.50 GPa218 ksiISO 527
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched  0.700 J/cm²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 0.700 J/cm²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 140 °C284 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C122 °FISO 75
Vicat Softening Point  150 °C
@Load 5.10 kg
302 °F
@Load 11.2 lb
Method B; ISO 306
 175 °C
@Load 1.02 kg
347 °F
@Load 2.25 lb
Method A; ISO 306
 
Descriptive Properties
ColorBlack

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik VESTAMID® NRG 1001 PA 12
Evonik VESTAMID® NRG 2101 PA 12
Evonik VESTAMID® NRG 3001 PA 12
Evonik VESTAMID® NRG 1003 PA 12
Evonik VESTAMID® NRG 4101 PA 12

PEVONIL270 / 196474

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.