MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Barlog Plastics KEBABLEND WR XB 111001/5 Wear Resistant POM Compound
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Homopolymer, Unreinforced

Material Notes: KEBABLEND /WR XB 111001/5 is a special compound based on POM that exhibits very good sliding properties and high wear resistance.

Properties: dimensionally stable, good chemical resistance, good gliding properties, good recovery behavior, High strength, High stiffness, High wear resistance, semi-crystalline

Typical areas of application: Sliding elements, Plain bearing, industrial goods, Bearing bushes, Rollers, Rotors, Transport chains, Gears

Industries: Automotive, Household appliances, Industry, Agriculture, Mechanical Engineering, Furniture industry, Sports & Recreation

Information provided by BARLOG plastics GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.50 g/cc0.0542 lb/in³ISO 1183-1
Water Absorption 0.300 %0.300 %ISO 62
Moisture Absorption 1.00 %1.00 %50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0180 cm/cm0.0180 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0210 cm/cm0.0210 in/inISO 294-4
Melt Flow 2.00 g/10 min2.00 g/10 minISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 45.0 MPa6530 psiISO 527-1
Elongation at Yield 9.00 %9.00 %ISO 527-1
Modulus of Elasticity 2.80 GPa406 ksiISO 527-1
Charpy Impact Unnotched 4.00 J/cm²19.0 ft-lb/in²ISO 179-1eU
Charpy Impact, Notched 0.500 J/cm²2.38 ft-lb/in²ISO 179-1eA
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmContact; IEC 60093
Surface Resistance 1.00e+15 ohm1.00e+15 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
Melting Point 166 °C331 °FISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 120 °C248 °FISO 75-1/-2
Flammability, UL94  HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
IEC 60695-11-10
 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
IEC 60695-11-10
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 210 °C356 - 410 °F
Mold Temperature 90.0 - 100 °C194 - 212 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Back Pressure 0.000 - 5.00 MPa0.000 - 725 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBARLO491 / 326565

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.