MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polyplastic Armamid® PA 6-1FR Nylon 6, Flame Retardant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced, Flame Retardant

Material Notes: Halogen and phosphor free

Information provided by PolyPlastic Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³ISO 1183
Linear Mold Shrinkage <= 0.0020 cm/cm<= 0.0020 in/in
Linear Mold Shrinkage, Flow 0.0090 - 0.012 cm/cm0.0090 - 0.012 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0090 - 0.012 cm/cm0.0090 - 0.012 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 80.0 MPa11600 psiISO 37
Elongation at Break 10 %10 %ISO 37
Flexural Strength 105 MPa15200 psiISO 178
Flexural Modulus 3.00 GPa435 ksiISO 178
Charpy Impact Unnotched NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.800 J/cm²
@Temperature 23.0 °C
3.81 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Dielectric Strength 25.0 kV/mm635 kV/inIEC 60243-1
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 185 °C365 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C167 °FISO 75
Flammability, UL94 V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in
Glow Wire Test 960 °C
@Thickness 1.60 mm
1760 °F
@Thickness 0.0630 in
IEC 60695-2-1
 
Processing PropertiesMetricEnglishComments
Melt Temperature 235 - 245 °C455 - 473 °F
Mold Temperature 80.0 °C176 °F
Drying Temperature 85.0 °C
@Time 7200 - 14400 sec
185 °F
@Time 2.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 6, 20% Glass Fiber Filled
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
LG Chemical LUMID GP2200A(W) PA6+GF20%, General Purpose
Polyplastic Armamid® PA6 GF 30-2HSM-902 Nylon, 30% Glass Filled
Polyplastic Armamid® PA6 GF 30 HS-901 Nylon, 30% Glass Filled

PPOLYP934 / 157161

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.