MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Rubaloy Rubaloy 703G NBR / PVC
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Product Information: Rubaloy – 703G is a non-staining, oil, ozone, abrasion, weather and flex resistant polymer using medium ACN (33%) content Acrylonitrile Butadiene Rubber and a special grade of Poly Vinyl Chloride Resin. This grade has improved extrusion rate, extrusion, moulding and surface finish. Rubaloy-703G is Pthalate free.

Processing Characteristics: Rubaloy – 703G is easily processible on conventional rubber processing/compounding machines. Very good filler and plasticizer absorption makes the compounding cycle quick, saving time and reducing cost. Warm mixing mill compounding is recommended for best results. Rubaloy–703G can easily withstand elevated compounding temperatures. Recommended plasticizers are DOP, DOA, DOS, DBP, TCR, CPO and other Aromatic Plasticizers. Paraffinic based softeners are not recommended.

Curing: Standard Sulphur or Peroxide curing systems are to be used. NBR/PVC is slow curing hence a high dosage of accelerators are recommended.

Applications: Gasoline Tubings and Hose Covers, Conveyor Belt covers, LPG Tubing, Auto Parts, Gaskets, Oil Seals, Oil Resistant and antistatic Shoe Soles, Rubber Sheets and Extruded Rubber Parts, Industrial Textile and Printing Rolls, Expanded Sheets for insulation, Auto weather strips etc.

Information provided by Rubaloy™

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.02 - 1.06 g/cc1.02 - 1.06 g/cc
Mooney Viscosity 70 - 80
@Temperature 100 °C
70 - 80
@Temperature 212 °F
ML 1+4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 55 - 6555 - 65
 
Descriptive Properties
ACN Content0.33
Extraction Percentage>5%
Polymer Ratio70:30
StabilizerNon-Staining

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRUBAL009 / 317273

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.