High viscosity, plasticized, heat and light stabilized PA12 Compound. VESTAMID® L2124 black 9.7507 is a plasticized, heat- and light- stabilized polyamide 12 compound for the extrusion of flexible tubing and hoses especially for oil and petrochemical applications. Tubing according to DIN 73 378, Type: PA 12-PHL. Properties of compounds based on PA 12 vary little with changing humidity due to low moisture absorption. Parts made of this semi-crystalline material are characterized by exceptional impact strength, low coefficient of friction and good chemical resistance. VESTAMID® L2124 natural colored is characterized by a high melt viscosity and good dimensional control during pipe extrusion. VESTAMID® L2124 is supplied as cylindrical granules, ready for processing, in moisture-proof bags. Pigmentation may affect values. Property data for dry samples unless otherwise noted. Information provided by Evonik. |