MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Solvay MIRACARE® BT Surfactant  (discontinued **)
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Optimized blend of anionic and amphoteric surfactants used in the formulation of low irritation shampoos, skin cleansers and baby care systems.

Chemical Name: AMPHOTERIC / ANIONIC SURFACTANT

INCI Name: Water, Disodium Lauroamphodiacetate, Sodium Trideceth Sulfate, Isopropyl Alcohol

CAS: 7732-18-5, 68608-66-2, 25446-78-0, 67-63-0

Available in: Asia Pacific, Europe, Latin America and North America

Applications: MIRACARE© BT is an optimized blend of amphoteric and anionic surfactants that is primarily used in the preparation of mild skin cleanser and hair shampoo formulations. In formulated systems, MIRACARE© BT functions as a mild foaming and cleansing agent.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 36 - 38 %
@Temperature 120 °C,
Time 7200 sec
36 - 38 %
@Temperature 248 °F,
Time 2.00 hour
Oven, 1 gram; RP-0540
pH 9.0 - 9.59.0 - 9.5RP-0420
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 4.0<= 4.0RP-0138
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
CompositionActive31.7-34.5%, %Active=%Solids-%Sodium Chloride
 Sodium Chloride3.5-4.3%, RP-0097

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WRHOD238 / 137469

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.