MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Latrobe Lescalloy® 52100 VAC-ARC High Performance Bearing Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Carbon Steel; High Carbon Steel

Material Notes: LESCALLOY 52100 VAC-ARC is a deep hardening alloy steel used for aircraft bearings and other high stressed parts where good rolling contact fatigue strength is required at operating temperatures below 400°F. This grade is produced by the vacuum-arc remelting process and offers greatly improved cleanliness and internal soundness over conventionally air melted bearing quality SAE 52100 steel.

Information Provided by Timken Latrobe Steel.

Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 7.80 g/cc7.80 g/cc
Density 7.75 g/cc0.280 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 45451/2" from quenched end
 66.566.51/8" from quenched end
Modulus of Elasticity 200 GPa29000 ksi
Modulus of Rigidity 82.7 GPa12000 ksi
Machinability 37 - 45 %37 - 45 %
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.6 µm/m-°C
@Temperature 38.0 - 260 °C
6.44 µin/in-°F
@Temperature 100 - 500 °F
 14.3 µm/m-°C
@Temperature 38.0 - 649 °C
7.94 µin/in-°F
@Temperature 100 - 1200 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 1.05 %1.05 %
Chromium, Cr 1.5 %1.5 %
Iron, Fe 96.8 %96.8 %
Manganese, Mn 0.35 %0.35 %
Silicon, Si 0.30 %0.30 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI E 52100 Steel (100Cr6, SUJ2, UNS G52986)
Crucible Steel AISI 52100 Alloy Steel
Latrobe Lescalloy® M50 VIM-VAR High Performance Bearing Steel
Sandvik Osprey SAE 52100 (100Cr6) Low Alloy Steel Powder
M50-NiL High Performance Carburizing Bearing and Gear Steel

NTIMK000 / 19348

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.